Product list
All product category names
- Flame retardant MCA series
- Flame retardant ADP series
- Flame retardant MPP series
- Flame retardant APP series
- New compound flame retardant series
- New environmental protection flame retardant series
- Wood special flame retardant series
- Special flame retardant for textiles series
- flame retardant masterbatch series
Contact us
MORE+Shouguang Puer Chemical Co. ,Ltd
Contact : Mr. Yang 13792680228
Sales Department: Ms Lai 0536-5291729
Fax :0536-5237306
International Department: Ms Li 13081694688
Website: www.puerchem.com
Email: sales@puerchem.com
Head Office Add: Building 22,Enterprise Headquarters Group,Shengcheng East Street,Shouguang,Shandong,262700.
Add: North of Jinguang Street ,Shouguang ,Shandong,China.(East of Xianxia Clothing Factory)
Add: 7 Chenming Industrial Park, Shengcheng Street, Shouguang City, Shandong Province
Add: PUER Flame Retardant New Materials Industrial Park, Dongming County, Shandong Province
Factory Website: www.yipunewmaterial.com
阻燃TPE/TPU线材特点及难点解决方案
热塑性弹性体TPE产品既具备传统交联硫化橡胶高弹性、耐老化、耐油性的优异性能,同时又具备普通塑料加工方便、方式广的特点。
但TPE加工经常会发生线材表面不光滑的问题,一般是温度调节和混料均匀度引起的,同时材料配方也影响重大。排除设备问题,调试合适温度,都很容易在反复测试中确定,剩下的就是选用合适的材料和具体配方控制。有经验的工程师清楚材料的物性和加工注意事项,那么起决定作用的就是材料,好的材料会事半功倍。通常来说,TPU线材相对TPE线材表面加工会更好。
线材出现的表面发白、冒油或成雾状,就是析出的具体表现。表面轻微发白的析出不会影响物理性能和电力性能,但表面冒油的材料在使用中容易发生脱落、掉皮,无法正常使用。另外析出也有轻重之分,好材料的析出是轻微的,短期内不易发生,即使发生也可轻易擦除。目前市场上没有哪家的材料能保证线材表面完全不析出,现在的技术水平还没有解决这个问题。
普尔研发团队针对这些问题进行反复研究,做出各种尝试,终于推出了新产品MC10。产品分散性能优异,粒径分布均匀,基本解决了传统MCA产品在TPE、TPU等线材使用过程中分散不好,易搭桥、易团聚,产生异色点的问题。该产品做的成品TPE/TPU线材,生产过程无挤渣,光滑度好,弹性也显著提升,杜绝了普通MCA的析出问题。
纳米级无卤阻燃剂MC10粒径D50小于0.5微米,具有粒径分布极其均匀而集中,分散性能优异的特点,在线材加工过程中搭配合适的螺杆组合,可以让线材外表更加光亮、细腻,大大优于传统MCA改性后粗糙的线材外观。
纳米级阻燃剂MC10还适用于纺丝级尼龙阻燃母粒、纺丝级PET阻燃母粒的制备。